Abstract

Polyamide 6 (PA6) is an important semi-crystalline engineering plastic widely used in electrical appliances, automotive materials, and other applications. However, PA6 is highly susceptible to moisture absorption, which can significantly alter its physicochemical properties. In this study, PA6 was synthesized via anionic ring-opening polymerization, and immersion tests were conducted in accordance with ISO 175:2010. The influence of environmental factors on the non-isothermal crystallization behavior of PA6 was investigated. The Mo equation was successfully employed to characterize the entire non-isothermal crystallization process. The obtained kinetic parameters provide valuable insights for predicting the performance of PA6 under practical conditions and serve as a reference for the modification and optimization of PA6.

References

[1] Li M, Qiu J, Yue Y, et al. The Preparation of Monomer Casting Polyamide 6/Thermotropic Liquid Crystalline Polymer Composite Materials with Satisfactory Miscibility. Polymers 2022; 14. DOI: 10.3390/polym14204355.

[2] Álvarez-Láinez ML and Palacio R JA. Correlations between thermal and tensile behavior with friction coefficient in copolyamides 6/12. Wear 2017; 372-373: 76-80. DOI: 10.1016/j.wear.2016.11.018.

[3] Zhang H-X, Park J-Y, Lee D-E, et al. Fabrication of PA6/MoS2 nanocomposites via melt blending of PA6 with PA6/PEG modified-MoS2 masterbatch. Polymer Bulletin 2022; 79: 10639-10652. DOI: 10.1007/s00289-021-04068-z.

[4] Yin X, Zhao X and Ye L. In situ‐induced epiphytic crystallization of MC PA6 by self‐assembled nucleator and reinforcing effect. Polymer International 2023; 72: 629-639. DOI: 10.1002/pi.6513.

[5] Skorupska M, Kulczyk M, Denis P, et al. Structural Hierarchy of PA6 Macromolecules after Hydrostatic Extrusion. Materials 2023; 16. DOI: 10.3390/ma16093435.

[6] Unnikrishnan V, Zabihi O, Li Q, et al. Multifunctional PA6 composites using waste glass fiber and green metal organic framework/graphene hybrids. Polymer Composites 2022; 43: 5877-5893. DOI: 10.1002/pc.27002.

[7] Liu H, Wang Z, Pan B, et al. Carbon felt/nitrogen-doped graphene/paraffin wax 3D skeleton regulated tribological performances of the MCPA6 composites: A novel strategy of oil embedding and transporting. Tribology International 2023; 184. DOI: 10.1016/j.triboint.2023.108440.

[8] Unal H and Mimaroglu A. Friction and wear performance of polyamide 6 and graphite and wax polyamide 6 composites under dry sliding conditions. Wear 2012; 289: 132-137. DOI: 10.1016/j.wear.2012.04.004.

[9] Rwei S-P, Ranganathan P, Chiang W-Y, et al. Synthesis of Low Melting Temperature Aliphatic-Aromatic Copolyamides Derived from Novel Bio-Based Semi Aromatic Monomer. Polymers 2018; 10. DOI: 10.3390/polym10070793.

[10] Hirai T, Onochi Y and Kawada J. Multifaceted property tailoring of polyamide 6 by blending miscible and immiscible components: ternary blends of polyamide 6/polyethylene terephthalate/phenol novolac. RSC Advances 2020; 10: 15132-15138. DOI: 10.1039/d0ra02344b.

[11] Carrascal I, Casado JA, Polanco JA, et al. Absorption and diffusion of humidity in fiberglass-reinforced polyamide. Polymer Composites 2005; 26: 580-586. DOI: 10.1002/pc.20134.

[12] Sun D, Li J, Pan Q, et al. The In Situ Polymerization and Characterization of PA6/LiCl Composites. Journal of Spectroscopy 2013; 2013: 1-4. DOI: 10.1155/2013/164275.

[13] Sambale AK, Stanko M, Emde J, et al. Characterisation and FE Modelling of the Sorption and Swelling Behaviour of Polyamide 6 in Water. Polymers 2021; 13. DOI: 10.3390/polym13091480.

[14] Oh K, Kim H and Seo Y. Effect of Diamine Addition on Structural Features and Physical Properties of Polyamide 6 Synthesized by Anionic Ring-Opening Polymerization of ε-Caprolactam. ACS Omega 2019; 4: 17117-17124. DOI: 10.1021/acsomega.9b01342.

[15] Lin H-M, Behera K, Yadav M, et al. Polyamide 6/Poly(vinylidene fluoride) Blend-Based Nanocomposites with Enhanced Rigidity: Selective Localization of Carbon Nanotube and Organoclay. Polymers 2020; 12. DOI: 10.3390/polym12010184.

[16] Manker LP, Hedou MA, Broggi C, et al. Performance polyamides built on a sustainable carbohydrate core. Nature Sustainability 2024; 7: 640-651. DOI: 10.1038/s41893-024-01298-7.

[17] Zhang C, Liu C, Zhao H, et al. Effect of nanoparticle and glass fiber on the hydrothermal aging of polyamide 6. Journal of Applied Polymer Science 2020; 137. DOI: 10.1002/app.49585.

[18] Sambale AK, Maisl M, Herrmann H-G, et al. Characterisation and Modelling of Moisture Gradients in Polyamide 6. Polymers 2021; 13. DOI: 10.3390/polym13183141.

[19] Dou Y, Mu X, Chen Y, et al. Effect of Composition on the Crystallization, Water Absorption, and Biodegradation of Poly(ε-caprolactam-co-ε-caprolactone) Copolymers. Polymers 2020; 12. DOI: 10.3390/polym12112488.

[20] Park M, Jang J-u, Park JH, et al. Enhanced Tensile Properties of Multi-Walled Carbon Nanotubes Filled Polyamide 6 Composites Based on Interface Modification and Reactive Extrusion. Polymers 2020; 12. DOI: 10.3390/polym12050997.

[21] Li Y, Nie D and Cai Z. The performance analysis of screw pump stator elastomers: Polyamide 6/hydrogenated nitrile blends: Mechanical, oil resistance and tribological properties. Polymer Testing 2023; 128. DOI: 10.1016/j.polymertesting.2023.108226.

[22] Heimrich M, Nickl H, Bönsch M, et al. Migration of Cyclic Monomer and Oligomers from Polyamide 6 and 66 Food Contact Materials into Food and Food Simulants: Direct Food Contact. Packaging Technology and Science 2015; 28: 123-139. DOI: 10.1002/pts.2094.

[23] Bomfim MVJ, Zamith HPS and Abrantes SMP. Migration of ɛ-caprolactam residues in packaging intended for contact with fatty foods. Food Control 2011; 22: 681-684. DOI: 10.1016/j.foodcont.2010.09.017.

[24] Sela R, Bychanok D, Padrez Y, et al. Electromagnetic properties of chloroprene rubber after long-term ultraviolet ageing, oil immersion and thermal degradation. Materials Research Express 2019; 6. DOI: 10.1088/2053-1591/ab1574.

[25] Bawase M, Chaudhari S and Thipse SS. Polymer/fuel interaction and properties of typical automotive fuel-system polymers exposed to methanol blended (M15) gasoline. Polymer Testing 2021; 97. DOI: 10.1016/j.polymertesting.2021.107141.

[26] Tormos B, Bermúdez V, Balaguer A, et al. Compatibility Study of Polyamide (PA6) with Lubricant Bases for Electric Vehicle Applications. Lubricants 2024; 12. DOI: 10.3390/lubricants12020054.

[27] He H, Wang X, Xu P, et al. Flower-like MnO2 nanoparticles modified thin film nanocomposite membranes for efficient organic solvent nanofiltration. Composites Communications 2023; 38. DOI: 10.1016/j.coco.2023.101515.

[28] Xu X, Shu X, Pei Q, et al. Effects of porosity on the tribological and mechanical properties of oil-impregnated polyimide. Tribology International 2022; 170. DOI: 10.1016/j.triboint.2022.107502.

[29] Kalácska G, Zsidai L, Keresztes R, et al. Effect of nitrogen plasma immersion ion implantation of polyamide-6 on its sliding properties against steel surface. Wear 2012; 290-291: 66-73. DOI: 10.1016/j.wear.2012.05.011.

[30] Durbin TD, Karavalakis G, Norbeck JM, et al. Material compatibility evaluation for elastomers, plastics, and metals exposed to ethanol and butanol blends. Fuel 2016; 163: 248-259. DOI: 10.1016/j.fuel.2015.09.060.

Downloads

Published

27-03-2025

Issue

Section

Articles

How to Cite

Zhang, X. (2025). The Effect of Hydrothermal Aging on the Non-Isothermal Crystallization Behavior of Polyamide 6. International Journal of Materials Science and Technology Studies, 3(2), 24-31. https://doi.org/10.62051/ijmsts.v3n2.04